Titanium Grade 7 Sheet & Plate
Titanium Grade 7 Sheet & Plate supplied to the specified dimensions, condition, tolerance, inspection and material-traceability requirements for industrial procurement.
- Material
- Titanium Grade 7 / UNS R52400
- Standard
- ASTM B265 / ASME SB265
- Product Form
- Sheet, plate and cut blanks; thickness, width, length, flatness and edge condition are confirmed by RFQ
- Documents
- MTC, inspection and heat/lot traceability
Product Detail
Product Introduction
Titanium Grade 7 Sheet & Plate is supplied for corrosion-resistant fabrication and precision manufacturing. The final purchase definition must identify the exact material designation, governing specification and revision, dimensions, condition, tolerances, tests and documentation; trade-name or cross-standard equivalence is not assumed.
When is Grade 7 plate preferred to Grade 2?
Selection answer: Grade 7 is a palladium-bearing commercially pure titanium grade selected to improve resistance in certain reducing or crevice-corrosion environments while retaining fabrication behavior broadly associated with CP titanium.
Selection boundary: The palladium addition does not make the material universally resistant. Media chemistry, concentration, contaminants, aeration, temperature and crevice geometry must be reviewed before selection.
RFQ data to confirm: Send process chemistry, concentration, operating and upset temperatures, fabrication and welding plan, thickness, dimensions, tests and certificate requirements.
Product Specifications
| Product | Titanium Grade 7 Sheet & Plate | Grade | Titanium Grade 7 / UNS R52400 |
|---|---|---|---|
| Standard | ASTM B265 / ASME SB265 | Size & Form | Sheet, plate and cut blanks; thickness, width, length, flatness and edge condition are confirmed by RFQ |
| Tolerance | Governing material standard or approved customer drawing | Supply Condition | Hot or cold rolled, annealed, pickled, blasted, brushed or polished as applicable |
| Inspection | MTC review, dimensional and surface inspection, heat/lot traceability, with PMI or applicable NDT when specified | Documents | MTC, heat/lot traceability and agreed inspection reports |
Send the complete material RFQ
Include grade, specification revision, dimensions, tolerance, quantity, condition, tests and destination.
Chemical Composition
Weight percent; maximum unless a range is shown. Titanium is the balance. The ordered specification and grade control.
| Grade / UNS | Principal Alloying Elements | Fe max | O max | C max | N max | H max | Ti |
|---|---|---|---|---|---|---|---|
| Grade 1 / R50250 | — | 0.20 | 0.18 | 0.08 | 0.03 | 0.015 | Balance |
| Grade 2 / R50400 | — | 0.30 | 0.25 | 0.08 | 0.03 | 0.015 | Balance |
| Grade 3 / R50550 | — | 0.30 | 0.35 | 0.08 | 0.05 | 0.015 | Balance |
| Grade 4 / R50700 | — | 0.50 | 0.40 | 0.08 | 0.05 | 0.015 | Balance |
| Grade 5 / R56400 | Al 5.50–6.75; V 3.50–4.50 | 0.40 | 0.20 | 0.08 | 0.05 | 0.015 | Balance |
| Grade 6 / R54520 | Al 4.00–6.00; Sn 2.00–3.00 | 0.50 | 0.20 | 0.08 | 0.05 | 0.015 | Balance |
| Grade 7 / R52400 | Pd 0.12–0.25 | 0.30 | 0.25 | 0.08 | 0.03 | 0.015 | Balance |
| Grade 9 / R56320 | Al 2.50–3.50; V 2.00–3.00 | 0.25 | 0.15 | 0.08 | 0.03 | 0.015 | Balance |
| Grade 12 / R53400 | Mo 0.20–0.40; Ni 0.60–0.90 | 0.30 | 0.25 | 0.08 | 0.03 | 0.015 | Balance |
| Grade 11 / R52250 | Pd 0.12–0.25 | 0.20 | 0.18 | 0.08 | 0.03 | 0.0125 | Balance |
| Grade 16 / R52402 | Pd 0.04–0.08 | 0.30 | 0.25 | 0.08 | 0.03 | 0.015 | Balance |
| Grade 17 / R52252 | Pd 0.04–0.08 | 0.20 | 0.18 | 0.08 | 0.03 | 0.0125 | Balance |
| Grade 19 / R58640 | Al 3.00–4.00; V 7.50–8.50; Cr 5.50–6.50; Mo 3.50–4.50; Zr 3.50–4.50 | 0.30 | 0.12 | 0.05 | 0.03 | 0.015 | Balance |
| Grade 23 / R56407 | Al 5.50–6.50; V 3.50–4.50 | 0.25 | 0.13 | 0.08 | 0.05 | 0.0125 | Balance |
Mechanical Properties – Annealed Material Reference
| Grade | Ultimate Tensile Strength min | 0.2% Yield Strength min | Elongation min |
|---|---|---|---|
| Grade 1 | 240 MPa | 170 MPa | 24% |
| Grade 2 | 345 MPa | 275 MPa | 20% |
| Grade 3 | 450 MPa | 380 MPa | 18% |
| Grade 4 | 550 MPa | 483 MPa | 15% |
| Grade 5 | 895 MPa | 828 MPa | 10% |
| Grade 6 | 828 MPa | 793 MPa | 10% |
| Grade 7 | 345 MPa | 275 MPa | 20% |
| Grade 9 | 620 MPa | 485 MPa | 15% |
| Grade 12 | 483 MPa | 345 MPa | 18% |
| Grade 11 | 240 MPa | 170 MPa | 24% |
| Grade 16 | 345 MPa | 275 MPa | 20% |
| Grade 17 | 240 MPa | 170 MPa | 24% |
| Grade 19 / Beta-C | Acceptance depends on solution treatment, aging condition, product form and section size; use the certified values required by the invoked product or aerospace specification. | ||
| Grade 23 | 860 MPa | 795 MPa | 10% |
Representative minima only. Product form, section size, heat treatment and the invoked specification determine the certified acceptance values.
Typical Physical Properties
| Grade | Density | Elastic Modulus | Thermal Expansion |
|---|---|---|---|
| Grade 1 | 4.51 g/cm³ | Approx. 103 GPa | Approx. 8.6 µm/m·K |
| Grade 2 | 4.51 g/cm³ | Approx. 105 GPa | Approx. 8.6 µm/m·K |
| Grade 3 | 4.51 g/cm³ | Approx. 105 GPa | Approx. 8.6 µm/m·K |
| Grade 4 | 4.51 g/cm³ | Approx. 105 GPa | Approx. 8.6 µm/m·K |
| Grade 5 | 4.43 g/cm³ | Approx. 114 GPa | Approx. 8.6 µm/m·K |
| Grade 6 | Approx. 4.48 g/cm³ | Approx. 110 GPa | Approx. 8.8 µm/m·K |
| Grade 7 | Approx. 4.51 g/cm³ | Approx. 105 GPa | Approx. 8.6 µm/m·K |
| Grade 9 | Approx. 4.48 g/cm³ | Approx. 105 GPa | Approx. 9.0 µm/m·K |
| Grade 12 | Approx. 4.54 g/cm³ | Approx. 103 GPa | Approx. 8.6 µm/m·K |
| Grade 11 | Approx. 4.51 g/cm³ | Approx. 103 GPa | Approx. 8.6 µm/m·K |
| Grade 16 | Approx. 4.51 g/cm³ | Approx. 105 GPa | Approx. 8.6 µm/m·K |
| Grade 17 | Approx. 4.51 g/cm³ | Approx. 103 GPa | Approx. 8.6 µm/m·K |
| Grade 19 / Beta-C | Approx. 4.82 g/cm³ | Condition-dependent; use certified engineering data | Condition-dependent; verify for design |
| Grade 23 | 4.43 g/cm³ | Approx. 114 GPa | Approx. 8.6 µm/m·K |
Typical engineering references, not inspection acceptance limits.
Certificates & Inspection Records

Services We Can Provide
Product Packaging
Sheet and plate surfaces are interleaved or wrapped as required, protected at edges and secured on pallets or in export cases with grade, heat and dimensional identification. Typical export packaging for the same physical product form is shown below; final packing is confirmed for each order.

Application Scenarios

Chemical processing equipment
Material grade, dimensions, condition and inspection must be matched to the application requirements.

Marine and desalination systems
Material grade, dimensions, condition and inspection must be matched to the application requirements.

Industrial fabrication and precision components
Material grade, dimensions, condition and inspection must be matched to the application requirements.
Specification & Selection Notes
Product-standard boundary
ASTM B265/B265M covers annealed titanium and titanium-alloy strip, sheet and plate and identifies Grade 7 as UNS R52400 unalloyed titanium with 0.12 % to 0.25 % palladium. The order should state the exact revision, Grade 7 / UNS R52400, sheet or plate form, final condition, dimensions and tolerances, flatness, surface, edge, quantity and documentation. Grade 7H shares UNS R52400 but has a higher guaranteed minimum tensile strength and is a distinct ordered grade designation.
Inspection and traceability
Verify Grade 7 / UNS R52400 heat identity, chemistry including palladium, tensile properties and test orientation, final condition, thickness, width and length, flatness, surface and edges, marking, MTC and heat/lot traceability. Additional corrosion testing, ultrasonic examination or customer witness must name the test method, sampling and acceptance criteria.
Selection boundary
Grade 7 is commonly evaluated where palladium-alloyed commercially pure titanium is required for a specific corrosion environment, but it is not a blanket upgrade for every chemical service. Process composition, concentration, contaminants, temperature, flow, crevice geometry, fabrication route and the approved design basis must be reviewed before choosing it over Grade 2 or Grade 12.
Technical FAQ
When should Grade 7 be considered instead of Grade 2?
Consider Grade 7 when the approved corrosion assessment specifically benefits from its palladium addition. Selection should be based on the actual process chemistry and temperature, not only on a general corrosion-resistance claim.
Are Grade 7 and Grade 7H interchangeable?
They share UNS R52400 and the same palladium range, but Grade 7H has a higher guaranteed minimum tensile strength. Use the grade designation required by the design and governing code.
What information is needed to quote Grade 7 sheet or plate?
Provide ASTM B265/B265M revision, Grade 7 / UNS R52400, sheet or plate form, condition, dimensions and tolerances, flatness, surface, edge, service chemistry and temperature, quantity, testing, MTC and destination.
FAQ
What information is required to quote Titanium Grade 7 Sheet & Plate?
Provide the titanium grade, product form, dimensional standard or drawing, thread or critical dimensions, quantity, surface treatment, mating parts, service conditions and required inspection documents.
Which standards apply to Titanium Grade 7 Sheet & Plate?
ASTM B265 / ASME SB265
How are Titanium Grade 7 Sheet & Plate inspected?
MTC review, dimensional and surface inspection, heat/lot traceability, with PMI or applicable NDT when specified
Leave Your Message
Related Technical Guides
Titanium Plate and Tube Sheet for Desalination
Review grade, equipment geometry, fabrication and inspection for seawater service.
Read technical guideHow to Choose a Titanium Grade
Compare grade, strength, corrosion environment and fabrication needs.
Read technical guideTitanium RFQ Checklist
Prepare dimensions, standards, tests and documentation.
Read technical guideComplete Titanium Product Guide
Compare titanium product forms and sourcing considerations.
Read technical guide