Grade 5 Ti-6Al-4V Titanium Sheet & Plate

Source Grade 5 Ti-6Al-4V titanium sheet and plate for aerospace and high-strength fabrication, with inspection and traceability.

Material
Grade 5 / Ti-6Al-4V / UNS R56400
Standard
ASTM B265; selected aerospace orders may reference AMS 4911
Supply
Annealed, hot rolled or cold rolled, pickled or blasted
Documents
MTC, inspection and heat/lot traceability
CONTACT US

Product Detail

Product Introduction

Source Grade 5 Ti-6Al-4V titanium sheet and plate for aerospace and high-strength fabrication, with inspection and traceability. Final supply is controlled by the grade, specification revision, dimensions, condition, tolerance, inspection and documentation stated on the approved order.

When should Grade 5 Ti-6Al-4V plate be used?

Selection answer: Grade 5 is an alpha-beta alloy chosen primarily for high strength-to-weight performance, fatigue-sensitive structures and machined components rather than as a general replacement for commercially pure corrosion-service plate.

Selection boundary: Its corrosion behavior, formability, heat treatment and weld requirements differ from Grade 2 or Grade 7. ASTM B265 and an aerospace specification such as AMS 4911 are not interchangeable purchase descriptions.

RFQ data to confirm: Specify the exact standard and revision, condition or heat treatment, thickness, direction-sensitive test requirements, ultrasonic testing if required, machining allowance and end use.

Product Specifications

ProductGrade 5 Ti-6Al-4V Titanium Sheet & PlateGradeGrade 5 / Ti-6Al-4V / UNS R56400
StandardASTM B265 covers annealed titanium strip, sheet and plate and identifies Grade 5 Ti-6Al-4V as UNS R56400. An aerospace material specification such as AMS 4911 may impose a different condition, testing, quality and documentation package; do not treat ASTM B265 and an AMS order as interchangeable.Size & FormSheet, plate and cut blanks; thickness and dimensions are confirmed per RFQ
ToleranceApplicable ASTM, AMS or customer drawingSupply ConditionAnnealed, hot rolled or cold rolled, pickled or blasted
InspectionVerify the exact standard and revision, Grade 5 / UNS R56400 heat identity, chemistry including interstitial limits, mechanical properties and test orientation, condition, thickness, width, length, flatness, surface, edges and marking. Define ultrasonic or penetrant examination, microstructure, grain direction, machining allowance and aerospace documentation only with the required method and acceptance criteria.DocumentsMTC, heat/lot traceability and agreed inspection reports

Additional Supply & Ordering Details

Useful, technically consistent information consolidated from earlier product pages.

Specification boundaryASTM B265 Grade 5 and AMS4911 Ti-6Al-4V are not interchangeable order descriptions. State the exact standard, revision, condition, product form and supplementary aerospace or project requirements.
Condition and directionDefine annealed or other approved condition, thickness, rolling direction and test orientation. Mechanical acceptance and forming behavior depend on product form, section and heat-treatment route.
Machining and fatigue dataProvide finished-part drawing, stock allowance, flatness, surface, edge condition, fatigue-critical surfaces and any restriction on thermal cutting or repair.
Inspection packageState chemistry and tensile reports, heat traceability, dimensions, surface, ultrasonic class when required, microstructure or aerospace documentation and third-party witness points.

Send the complete material RFQ
Include grade, specification revision, dimensions, tolerance, quantity, condition, tests and destination.

Request a Quotation

Chemical Composition

Weight percent; maximum unless a range is shown. Titanium is the balance. The ordered specification and grade control.

Grade / UNSPrincipal Alloying ElementsFe maxO maxC maxN maxH maxTi
Grade 5 / R56400Al 5.50–6.75; V 3.50–4.500.400.200.080.050.015Balance

Mechanical Properties – Annealed Material Reference

GradeUltimate Tensile Strength min0.2% Yield Strength minElongation min
Grade 5895 MPa828 MPa10%

Representative minima only. Product form, section size, heat treatment and the invoked specification determine the certified acceptance values.

Typical Physical Properties

GradeDensityElastic ModulusThermal Expansion
Grade 54.43 g/cm³Approx. 114 GPaApprox. 8.6 µm/m·K

Typical engineering references, not inspection acceptance limits.

Certificates & Inspection Records

SAKY ALLOY quality management system certificate

Services We Can Provide

Specification ReviewGrade, revision, condition and supplementary requirements.
Cut-to-Size SupplyDimensions, machining allowance and tolerances by review.
InspectionDimensions, surface, chemistry and mechanical documentation.
Testing OptionsPMI, UT, PT or other agreed testing where applicable.
TraceabilityMTC, heat/lot identity and inspection records.
Export SupportProtected packing, labels and shipping documents.

Product Packaging

Sheet and plate surfaces are interleaved or wrapped as required, protected at edges and secured on pallets or in export cases with grade, heat and dimensional identification. Typical export packaging for the same physical product form is shown below; final packing is confirmed for each order.

Titanium plates and sheets packed with surface and edge protection

Application Scenarios

Chemical processing plant with industrial process piping

Aerospace structures

Material grade, dimensions, condition and inspection must be matched to the application requirements.

Wind turbines and solar panels at a renewable energy site

Motorsport and marine parts

Material grade, dimensions, condition and inspection must be matched to the application requirements.

Cargo vessel moored for marine service

High-strength fabricated components

Material grade, dimensions, condition and inspection must be matched to the application requirements.

FAQ

Is ASTM B265 Grade 5 plate the same as AMS 4911 plate?

No. Both may describe Ti-6Al-4V flat product, but the governing specification, revision, condition, test orientation, quality controls and documentation can differ. The purchase order must name the required specification.

Can Grade 5 plate be substituted for Grade 23 ELI plate?

Not automatically. Grade 23 has extra-low-interstitial chemistry and may be ordered under a different UNS or application specification. Substitution requires engineering and specification approval.

What information is needed to quote Grade 5 sheet or plate?

Provide ASTM B265, AMS 4911 or the exact project specification and revision, Grade 5 / UNS R56400, sheet, plate or cut blank, thickness, width, length, condition, surface, flatness, test orientation, NDT, quantity, MTC and traceability.

Leave Your Message

Related Technical Guides

WhatsApp