Titanium Tube Eddy Current Reports: Reference Setup and Disposition

Review titanium tube eddy current reports by lot identity, reference setup, examined coverage and disposition.

  • Standards-aware sourcing guidance
  • Grade and application comparisons
  • Inspection and RFQ considerations

An eddy current report should connect the delivered tube lot to a defined examination setup, reference response, examined extent and disposition. A statement that material was tested does not explain the acceptance basis or establish leak tightness.

Start with the inspection purpose

Separate new-tube manufacturing acceptance from an in-service bundle survey. Their identification systems, access conditions and decision criteria can differ. Record the governing purchase specification, approved procedure and applicable edition before interpreting results.

Follow the evidence chain

Review pointEvidence to requestQuestion it resolves
Tube identityHeat or lot, grade, dimensions and manufacturing routeDoes this report apply to the delivered material?
Reference setupReference identification, relevant geometry and documented settingsWhat response was the examination compared against?
CoverageQuantity and extent examined, inaccessible areas and limitationsWhat was actually inspected?
ResultsTraceable indications and the stated evaluation basisHow was each relevant result classified?
DispositionAcceptance, segregation, retest or other approved actionWhich pieces are released?

A reference response is not a universal flaw guarantee

Confirm that the reference and examination procedure are appropriate to the tube being supplied. Do not turn a response threshold into a guaranteed detectable flaw size without a qualified basis. A different material, geometry or examination arrangement needs its own assessment.

An in-service sample report can illustrate useful organization, but its damage categories, percentage-wall estimates and repair recommendations must not be copied into a new titanium-tube acceptance specification.

Close unexplained results before release

If identification, coverage or disposition is missing, request a corrected report or a documented clarification tied to the same lot. Keep retest results and their reason connected to the original record. A pass statement alone should not close an unresolved identification discrepancy.

Eddy current examination and leak testing answer different questions. Confirm separately which pressure or leak examination the governing order requires; do not describe one as automatically replacing the other.

For the product scope, review the B338, B861 and B862 comparison before defining the examination documents.