Titanium Socket Weld Flange

Titanium Socket Weld Flange supplied by grade, material standard, nominal size, pressure class, facing, bore, bolt pattern, connection details, inspection and documentation.

Grades
Grade 2, Grade 5, Grade 7, Grade 12 or specified grade
Material
ASTM B381 / ASME SB381 as applicable
Dimensions
ASME B16.5 or approved EN/DIN/JIS/customer drawing
Documents
MTC, dimensions and heat/lot traceability
CONTACT US

Product Detail

Product Introduction

Titanium Socket Weld Flange is a forged and machined titanium piping component identified by its internal socket and shoulder for pipe insertion. Material grade, dimensional standard, nominal size, pressure class, facing, mating component and service conditions must be reviewed together.

How should a titanium socket weld flange be ordered?

Selection answer: A socket weld flange receives the pipe end in a controlled socket and uses a fillet weld. The socket bore, counterbore, pipe OD, insertion gap and connected-pipe schedule must be coordinated.

Selection boundary: The internal crevice and fillet-weld geometry can affect corrosion, fatigue and cleanliness. Suitability must be confirmed by the piping code and service review, especially for aggressive media or cyclic duty.

RFQ data to confirm: Provide grade, NPS, class, facing, pipe schedule, socket dimensions, insertion-gap requirement, weld procedure, medium, design pressure and temperature, NDE, quantity and documents.

Product Specifications

ProductTitanium Socket Weld FlangeGradeTitanium Grade 2, Grade 5, Grade 7, Grade 12 or specified alloy
StandardASTM B381 / ASME SB381 may govern titanium-alloy forgings; ASME B16.5 or an approved EN, DIN, JIS or project standard may govern dimensions, pressure class and facing. The applicable piping code and project specification control selection and rating.Size & FormNPS/DN and Class/PN according to the specified dimensional standard or customer drawing
ToleranceApplicable material/dimensional standard and order-defined bore, hub, facing, bolt circle, hole and connection tolerancesSupply ConditionForged and machined with protected sealing faces, individual identification and reinforced export-case packing
InspectionMTC and heat traceability, PMI when specified, nominal size and pressure class, OD and thickness, bore and connection geometry, bolt circle and holes, facing and surface finish, visual inspection and supplementary NDE when required.DocumentsMTC, heat/lot traceability and agreed inspection reports

Additional Supply & Ordering Details

Useful, technically consistent information consolidated from earlier product pages.

Connection functionA socket-weld flange receives the pipe end in a machined socket and uses an external fillet weld. Socket depth, pipe setback and bore alignment are essential fabrication controls.
Critical dimensionsState NPS, class, facing, dimensional standard, socket bore and depth, through bore, pipe OD and wall, face finish, bolt drilling and grade.
Fabrication interfaceDefine pipe insertion gap, joint cleaning, filler, shielding and qualified fillet-weld procedure. Review crevice and fatigue implications for the intended service.
Inspection focusInspect socket diameter and depth, bore alignment, facing, flange thickness, bolt drilling, surface and material traceability; add PT or weld inspection for the completed joint as specified.

Send the complete material RFQ
Include grade, specification revision, dimensions, tolerance, quantity, condition, tests and destination.

Request a Quotation

Chemical Composition

Weight percent; maximum unless a range is shown. Titanium is the balance. The ordered specification and grade control.

Grade / UNSPrincipal Alloying ElementsFe maxO maxC maxN maxH maxTi
Grade 2 / R504000.300.250.080.030.015Balance
Grade 5 / R56400Al 5.50–6.75; V 3.50–4.500.400.200.080.050.015Balance
Grade 7 / R52400Pd 0.12–0.250.300.250.080.030.015Balance
Grade 12 / R53400Mo 0.20–0.40; Ni 0.60–0.900.300.250.080.030.015Balance

Mechanical Properties – Annealed Material Reference

GradeUltimate Tensile Strength min0.2% Yield Strength minElongation min
Grade 2345 MPa275 MPa20%
Grade 5895 MPa828 MPa10%
Grade 7345 MPa275 MPa20%
Grade 12483 MPa345 MPa18%

Representative minima only. Product form, section size, heat treatment and the invoked specification determine the certified acceptance values.

Typical Physical Properties

GradeDensityElastic ModulusThermal Expansion
Grade 24.51 g/cm³Approx. 105 GPaApprox. 8.6 µm/m·K
Grade 54.43 g/cm³Approx. 114 GPaApprox. 8.6 µm/m·K
Grade 7Approx. 4.51 g/cm³Approx. 105 GPaApprox. 8.6 µm/m·K
Grade 12Approx. 4.54 g/cm³Approx. 103 GPaApprox. 8.6 µm/m·K

Typical engineering references, not inspection acceptance limits.

Certificates & Inspection Records

SAKY ALLOY quality management system certificate

Services We Can Provide

Specification ReviewGrade, revision, condition and supplementary requirements.
Cut-to-Size SupplyDimensions, machining allowance and tolerances by review.
InspectionDimensions, surface, chemistry and mechanical documentation.
Testing OptionsPMI, UT, PT or other agreed testing where applicable.
TraceabilityMTC, heat/lot identity and inspection records.
Export SupportProtected packing, labels and shipping documents.

Product Packaging

Machined faces, bores and bevels are protected with covers or wrapping. Flanges are separated by grade, size and heat, then secured in reinforced export cases with traceability labels. Typical export packaging for the same physical product form is shown below; final packing is confirmed for each order.

Titanium flanges packed with sealing faces protected for shipment

Application Scenarios

Chemical processing plant with industrial process piping

Small-bore welded piping where the piping specification permits socket-weld joints

Material grade, dimensions, condition and inspection must be matched to the application requirements.

Wind turbines and solar panels at a renewable energy site

Chemical processing and corrosion-resistant piping

Material grade, dimensions, condition and inspection must be matched to the application requirements.

Cargo vessel moored for marine service

Marine, desalination and industrial equipment connections

Material grade, dimensions, condition and inspection must be matched to the application requirements.

FAQ

Does ASTM B381 define flange pressure class and dimensions?

No. ASTM B381 primarily covers titanium forgings. State the separate dimensional standard, size, class or PN, facing and project requirements.

Which titanium grade should be selected?

Grade selection depends on service chemistry, temperature, strength, mating materials, fabrication and the governing project specification.

What information is required for quotation?

Provide grade, material and dimensional standards, size, class/PN, facing, bore or connection details, quantity, NDE and certificates.

Leave Your Message

Related Technical Guides

WhatsApp